Database of Steel and Alloy (Marochnik)

en
HOME STANDARDS METALS SEARCH BULLETIN BOARD GRADING EDUCATION IN UKRAINE CONTACTS
 
(495)
(495)
Metals -> Structural steel -> Normal quality structural carbon steel

Characteristics of the material VSt5sp   ( VSt5sp,   ВСт5сп ).

Material : VSt5sp   ( VSt5sp,   ВСт5сп )
Substitute: Ст6сп, ВСт4сп
Classification : Normal quality structural carbon steel


Chemical composition in % of the material VSt5sp   ( VSt5sp,   ВСт5сп ) .
C Si Mn Ni S P Cr Cu As
0.28 - 0.370.15 - 0.350.5 - 0.8max   0.3max   0.05max   0.04max   0.3max   0.3max   0.08


Temperature of critical points of the grade VSt5sp   ( VSt5sp,   ВСт5сп ).
Ac1 = 730 ,      Ac3(Acm) = 825 ,       Ar3(Arcm) = 815 ,       Ar1 = 690


Mechanical properties under Т=20oС of the material VSt5sp   ( VSt5sp,   ВСт5сп ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging 100 - 300 longitudinal 350 175 24 50590Normalizing
Forging 300 - 500 longitudinal 350 175 22 45540Normalizing
Forging 500 - 800 longitudinal 350 175 20 40490Normalizing


Physical properties of the material VSt5sp   ( VSt5sp,   ВСт5сп ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.98          
100 1.96          
200 1.91          
300 1.85          
400 1.64          
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material VSt5sp   ( VSt5sp,   ВСт5сп ) .
  Weldability: limited weldability.
 Flakes : not predisposed
Temper brittleness: not predisposed



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user