Metals -> Structural steel -> Low alloy structural steel for welding construct

Characteristics of the material 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ).

Material : 20KHG2TS   ( 20HG2TS,   20ХГ2Ц )
Classification : Low alloy structural steel for welding construct


Chemical composition in % of the material 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ) .
C Si Mn Ni S P Cr Cu Zr
0.19 - 0.260.4 - 0.71.5 - 1.9max   0.3max   0.045max   0.0450.9 - 1.2max   0.30.05 - 0.14


Temperature of critical points of the grade 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ).
Ac1 = 770 ,      Ac3(Acm) = 835 ,       Ar3(Arcm) = 740 ,       Mn = 345


Mechanical properties under Т=20oС of the material 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rebar Ж 10 - 18   900 600 6    


Physical properties of the material 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20            
100   12.3        
200   12.3        
300   12.5        
400   13.1        
500   13.5        
600   13.9        
700   14.2        
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material 20KHG2TS   ( 20HG2TS,   20ХГ2Ц ) .
  Weldability: without limitations.



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-