Characteristics of the material VT6   ( ВТ6 ).

Material : VT6   ( ВТ6 )
Classification : Titanium wrought alloy


Chemical composition in % of the material VT6   ( ВТ6 ) .
Fe C Si V N TiAl Zr OH Impurity
max   0.3max   0.1max   0.153.5 - 5.3max   0.0586.485 - 91.25.3 - 6.8max   0.3max   0.2max   0.015 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС of the material VT6   ( ВТ6 ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar     900-1100  8-2020-45400Annealing
Bar     1100-1250  6 20300Hardening and ageing
Die     950-1100  10-1335-60400-800Annealing


    Brinell hardness of the material   VT6   ( ВТ6 )   (quenching, ageing ,     Bar HB 10 -1= 293 - 361   MPa
    Brinell hardness of the material   VT6   ( ВТ6 )   (annealing) ,     Die HB 10 -1= 255 - 341   MPa


Physical properties of the material VT6   ( ВТ6 ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.15   8.37 4430   1600
100   8.4 9.21     1820
200   8.7 10.88   0.586 2020
300   9 11.7   0.67 2120
400   10 12.56   0.712 2140
500     13.82   0.795  
600     15.49   0.879  
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material VT6   ( ВТ6 ) .
  Weldability: without limitations.



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-