Characteristics of the material 50KH   ( 50H,   50Х ).

Material : 50KH   ( 50H,   50Х )
Substitute: 40Х, 45Х, 50ХН, 50ХФА
Classification : Alloy structurall steel


Chemical composition in % of the material 50KH   ( 50H,   50Х ) .
C Si Mn Ni S P Cr Cu
0.46 - 0.540.17 - 0.370.5 - 0.8max   0.3max   0.035max   0.0350.8 - 1.1max   0.3


Temperature of critical points of the grade 50KH   ( 50H,   50Х ).
Ac1 = 720 ,      Ac3(Acm) = 770 ,       Ar3(Arcm) = 693 ,       Ar1 = 660 ,       Mn = 250


Mechanical properties under Т=20oС of the material 50KH   ( 50H,   50Х ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging to 100   590 345 18 45590Normalizing
Forging 100 - 300   590 345 17 40540Normalizing
Forging 300 - 500   590 345 14 38490Normalizing
Forging 500 - 800   590 345 12 38390Normalizing
Bar Ж 25   1080 885 9 40390Guenching 830oC, oil, Drawing 520oC, water,


    Brinell hardness of the material   50KH   ( 50H,   50Х )   (annealing) ,       HB 10 -1= 229   MPa


Physical properties of the material 50KH   ( 50H,   50Х ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.07     7820    
100   12.8        
200   13        
300   13.8        
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material 50KH   ( 50H,   50Х ) .
  Weldability: hard weldability.
 Flakes : predisposed
Temper brittleness: predisposed



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-