Characteristics of the material 20KH23N13   ( 20H23N13,   20Х23Н13 ).

Material : 20KH23N13   ( 20H23N13,   20Х23Н13 )
Classification : High alloy high-temperature steel


Chemical composition in % of the material 20KH23N13   ( 20H23N13,   20Х23Н13 ) .
C Si Mn Ni S P Cr Ti Cu
max   0.2max   1max   212 - 15max   0.025max   0.03522 - 25max   0.2max   0.3


Mechanical properties under Т=20oС of the material 20KH23N13   ( 20H23N13,   20Х23Н13 ) .
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar Ж 60   490 295 35 50 Guenching 1100 - 1150oC, air,
Sheet thin     540   35   Guenching 1100 - 1150oC,Cooling air,


Physical properties of the material 20KH23N13   ( 20H23N13,   20Х23Н13 ) .
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.07     7820    
100   14.9   7790 538  
200   15.7 17      
300   16.6 19      
400   17.1 21      
500   17.5 23      
600   17.8 24 7580    
700   18.2 27      
800     29 7480    
900     31      
T E 10- 5 a 10 6 l r C R 10 9


Technological properties of the material 20KH23N13   ( 20H23N13,   20Х23Н13 ) .
  Weldability: limited weldability.
Temper brittleness: predisposed



Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others).
Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader

Top

©   2003 - 2009   All rights reserved.       About program.
The entire risk as to use of the Database of Steel and Alloy (Marochnik) content is assumed by you the user

Информация взята с сайта Марочник стали и сплавов


Главная | Новости | Марочник сталей | Контакты | Обратная связь
© 2002 - 2009 Мосспецсталь. Все права защищены
 
-12345-