Chemical composition in % of the material 25G ( 25G, 25Г ) .
C
Si
Mn
Ni
S
P
Cr
Cu
0.22 - 0.3
0.17 - 0.37
0.7 - 1
max 0.3
max 0.035
max 0.035
max 0.3
max 0.3
Temperature of critical points of the grade 25G ( 25G, 25Г ).
Ac1 = 723 , Ac3(Acm) = 820
Mechanical properties under Т=20oС of the material 25G ( 25G, 25Г ) .
Assortment
Dimension
Direct.
sв
sT
d5
y
KCU
Heat treatment
-
mm
-
MPa
MPa
%
%
kJ / m2
-
Blank
to 25
500
300
22
50
Guenching 880oC, water, Drawing 560oC, air,
Brinell hardness of the material 25G ( 25G, 25Г ) (annealing) ,
HB 10 -1= 197 MPa
Specification :
Mechanical properties :
sв
- Tensile strength , [MPa]
sT
- Yield stress, [MPa]
d5
- Specific elongation at fracture , [ % ]
y
- Reduction of area , [ % ]
KCU
- Impact strength , [ kJ / m2]
HB
- Brinell hardness , [MPa]
Database of steels and alloys (Marochnik) contains information about chemical composition and properties of 1500 steels and alloys (stainless steel, alloy steel, carbone steel, structural steel, tool steel, cast iron, aluminum alloy, titanium alloy, copper alloy, nickel alloy, magnesium alloy and others). Helpfull for specialists in material technology, structural engineer, mechanical engineer, metallurgy and metal trader